Development and experimental study of copper selenide based thermo-electric material by the method of powder metallurgy
Keywords:
Thermoelectric Materials, Nano Scale, Green Synthesis, Figure of MeritAbstract
Copper Selenide is one of the promising single crystal thermoelectric material for power generation in low temperature range 300 - 360 K. Universal testing machine is used for pressing the Nano powder to obtain the Nano bulk samples. By using X-ray diffraction (XRD) and scanning electronic microscope (SEM) identified the structure and phase composition. This study shown that 150 kN pressing force in sample without carbon nano tubes showed ZT=1.2 at a temperature of 322K. It is also shown that thermal conductivity and power factor is mainly influencing the value of thermoelectric efficiency of the studied materials.
Metrics
Downloads
Published
How to Cite
Issue
Section
License
All the articles published in Manufacturing Technology Today (MTT) Journal are held by the Publisher. Central Manufacturing Technology Institute (CMTI) as a publisher requires its authors to transfer the copyright prior to publication. This will permit CMTI to reproduce, publish, distribute, and archive the article in print and electronic form and also to defend against any improper use of the article.